This article explains how demand for UV protective glass for valuable art objects and historical furnishings has increased. German-based Glashutte Lamberts Waldsassen has developed the first UV protective glass that can be mouth blown, "restauro-UV" in collaboration with Dr Drexler Glasswervice and the IGR Institute for Glass and Raw Materials Technology.