Tin Coatings For Glass

Cardinal Glass Coatings is providing glass companies with a coating system that includes hot end coating chemicals and equipment, cold end coatings chemicals and equipment, fume extraction and scrubbing equipment, and technical advice and training of plant personnel. The hot end coating is called Superglaze, and is a high-purity monobutyltin trichloride specifically prepared for the glass container industry. It includes a patented stabilizer that inhibits crystal formation in humid conditions. The equipment used in the coating systems are produced by Vidromecanica of Portugal. Cardinal Glass Coatings can be contacted on tel: (USA) 001 803 779 3795. (whole item)

Author
Un-named
Origin
Unknown
Journal Title
American Glass Review 119 4 Jan-Feb 1999 16
Sector
Container glass
Class
C 1318

Request article (free for British Glass members)

Tin Coatings For Glass
American Glass Review 119 4 Jan-Feb 1999 16
C 1318
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.