Thermodynamic Behaviour Of The Non-Bridging Oxygen-Free Glass System Xag2O.(2-X)Na2O.2Al2O3.3Sio2.B2O3 In Contact With Nitrate Melts.

Equilibrium data for the Na+/Ag+ ion exchange at 375 C between the glass which is free of non-bridging oxygen and the nitrate melts are analysed in two different ways.

Author
C Kaps
Origin
Friedrich-Schiller-Universitat, Jena
Journal Title
Glastechnische Berischte 1991 64 235 - 240
Sector
Special Glass
Class
S 591

Request article (free for British Glass members)

Thermodynamic Behaviour Of The Non-Bridging Oxygen-Free Glass System Xag2O.(2-X)Na2O.2Al2O3.3Sio2.B2O3 In Contact With Nitrate Melts.
Glastechnische Berischte 1991 64 235 - 240
S 591