Tempered glass hollowware is becoming more popular due to its better resistance to thermal and mechanical shock. This growth has led Vidromecanica to develop better tempering technology and equipment to offer flexibility, quality and high production rates, developed by its engineering division with its test laboratories. In this article, the author discusses the options.