Tempered Glass In Building (In French)

Tempered glass is being used more and more in buildings because of its mechanical strength, and to improve security in case of accidental breakage. However, tempering induces permanent stresses in glass. Treatment requirements (heating and cooling) are very important parameters.

Author
V Lieffrieg
Origin
Glaverbel, Belgium
Journal Title
Verre 7 5 2001 36-42