Taking The Heat Out Of In-House Cullet

Scraper conveyors have eliminated one of the most unpleasant tasks in the glassworks. At the same time they have simplified the recycling of hot waste glass.

Author
H Moser
Origin
Zippe Ind Gmbh, Germany
Journal Title
Glass Industry 81 2 2000 9-10, 14
Sector
Container glass
Class
C 1531

Request article (free for British Glass members)