Swedish Glass Packaging Trends

The activities of the PLM group are reviewed. Production from Sweden has reached almost 100,000/tpa. In 1998 green glass imports of 90,000 were reported, with clear glass imports standing at around 60,000 tonnes.

Author
A AASE
Origin
PLM GLASS SWEDEN
Journal Title
Glass November 1998 443-444
Sector
Container glass
Class
C 152