Submixture Model To Predict Nepheline Precipitation In Waste Glasses

High-alumina high-level waste (HLW) glasses are prone to nepheline precipitation during canister-centerline cooling (CCC). If sufficient nepheline forms, the chemical durability of the glass will be significantly impacted. Overly conservative constraints have been developed and used to avoid the deleterious effects of nepheline formation in US HLW glasses. The constraints used have been shown to significantly limit the loading of waste in glass at Hanford and therefore the cost and schedule of cleanup. A 90-glass study was performed to develop an improved understanding of the impacts of glass composition on the formation of nepheline during CCC. The CCC crystallinity data from these glasses were combined with 657 glasses found in the literature. The trends showed significant effects of Na2O, Al2O3, SiO2, B2O3, CaO, Li2O, and potentially K2O on the propensity for nepheline formation. A pseudo-ternary submixture model was proposed to identify the glass composition region prone to nepheline precipitation.

Author
J D Vienna Et Al
Origin
Unknown
Journal Title
Int J Appl Glass Sci 8 2017 143-157
Sector
Special Glass
Class
S 4385

Request article (free for British Glass members)

Submixture Model To Predict Nepheline Precipitation In Waste Glasses
Int J Appl Glass Sci 8 2017 143-157
S 4385
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.