Sublimation Problem Solving

Sublimation printing uses a full spectrum of vibrant colors to provide durable decorations on a variety of surfaces. While sublimation first became popular for printing on polyester T-shirts, recent advances in sublimation-friendly coatings for other materials have extended this method of transferring sharp and colorful images to wood, metal_and ceramic. With the availability of inexpensive computer systems for digital graphics, sublimation is becoming the easiest and fastest way to make personalized products. To see the article please goto: www.ceramicindustry.com/CDA/ArticleInformation/features/BNP__Features__I...

Author
S A Shah
Origin
Unknown
Journal Title
Ceramic Industry Web Article: 2001
Sector
Enamels
Class
E 122

Request article (free for British Glass members)

Sublimation Problem Solving
Ceramic Industry Web Article: 2001
E 122
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.