Study Of Barium Borovanadate Glasses Containing Iron. Part 2.Electron Paramagnetic Resonance, Infrared Spectrascopic, And Dc Resistivity Studies

A number of borovanadate, barium vanadate and barium borovanadate amorphous systems have been examined. The variations in electrical resistivity and activation energy with composition were explained on the basis of the conclusions derived from the structural studies.

Author
T K Bansal, R G Mendiratta
Origin
Indian Institute Of Technology, Delhi
Journal Title
Phys Chem Glasses 1987 28 6 242-249
Sector
Special Glass
Class
S 51

Request article (free for British Glass members)

Study Of Barium Borovanadate Glasses Containing Iron. Part 2.Electron Paramagnetic Resonance, Infrared Spectrascopic, And Dc Resistivity Studies
Phys Chem Glasses 1987 28 6 242-249
S 51