Study Of Barium Borovanadate Glasses Containing Iron. Part 1. X-Ray, Density, Differential Thermal Analysis, And Mossbauer Studies

Systematic studies have shown that the addition of boric oxide to vanadium pentoxide results in inceased glass-forming ability and an increase in the barium oxide content results in an increase in the density of these glasses.