The Structure Of Rhenium-Containing Sodium Alumino (Iron) Phosphate Glasses

The phase composition, structure and rhenium (technetium surrogate) speciation in sodium aluminium (iron) phosphate glasses synthesized under oxidizing and reducing conditions were examined using XRF, SEM, Fourier transform infrared, Raman, and X-ray absorption near edge structure spectroscopic methods.

Author
S V Stefanovsky Et Al
Origin
Frumkin Inst Phys Chem, Moscow, Russia
Journal Title
Appl Glass Sci 10 October 2019 479-487