Structural Variability And Dissolution Characteristics Of Rf Magnetron Sputtered Ion-Doped Phosphate Based Glass Coatings

Resorbable phosphate based glasses (PBG) can be tailored to deliver a controlled release of therapeutic ions, and have been applied as thin-film coatings to facilitate osseointegration of orthopaedic implants.