Structural Studies Of Glasses In The System Sro-B2O3-Al2O3-Tio2

Two series of glasses with widely varying strontia and titania contents were prepared. Nuclear magnetic resonance, Raman, and infrared spectroscopy were used to study the structure of the glasses in comparison with crystalline borates and titanates.