Structural Investigation And Properties Of Gallium Zinc Phosphate Glasses

Phosphate glasses, especially glasses based on zinc-phosphate, are being intensively studied during recent years because they provide some unique physical properties compared to silicate glasses, such as low melting temperature, high coefficient of thermal expansion and low optical dispersion. The introduction of various metal oxides results in variability of their physical and chemical properties, gallium trioxide has received attention because of improving chemical durability and of antibacterial properties. The aim of this work was to study the effect of substitution of zinc by gallium on some physicochemical properties of phosphate glasses, as well as on their structure.

Author
J Holubova Et Al
Origin
University Pardubice, Czech Republic
Journal Title
13Th Symp Eu Soc Of Glass Science 2016 109
Sector
Special Glass
Class
S 4325

Request article (free for British Glass members)

Structural Investigation And Properties Of Gallium Zinc Phosphate Glasses
13Th Symp Eu Soc Of Glass Science 2016 109
S 4325
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.