Stress Relaxation And Refractive Index Change Of As2S3 In Compression Molding

As2S3 is one of the chalcogenide glasses that have attracted increasing interests for compression molding applications. This paper is aimed to evaluate the stress relaxation behaviour of As2S3 above its glass transition temperature and calculate its refractive index change during cooling.

Author
J Zhou Et Al
Origin
University Sci & Technol, Hefei, China
Journal Title
Appl Glass Sci 8 2017 255-265
Sector
Special Glass
Class
S 4406