Spectrophotometric Determination Of Copper In Glass After Extraction Of Copper Dithizonate On Polyurethane Foam

This paper covers the selective sorption and preconcentration of copper (II) dithizonate complex on unloaded polyurethane foam, thereby developing a spectrophotometric method for the determination of copper present in the glass system.

Author
D Kundu, S K Roy
Origin
Cgcri, India
Journal Title
Glass Technology 34 1 February 1993 33-36