A Solution To The Problem Of Zircon Cords

Today, consumers expect glass packaging to be as perfect as the products they contain. Therefore, manufacturers need to solve quality problems, such as zircon cords. In this article, a continuous drainage system, like Sorg's "Contidrain", can eliminate contaimated glass from the furnace bottom before it reaches the extraction flow.