[Solar] Pv Module Completes Mechanical Load Test

According to Tobias Neff, the TPedge module, jointly developed by Bystronic glass and the Fraunhofer Institute for Solar Energy Systems ISE, has successfully completed mechanical load and hail impact tests in accordance with IEC 61215.