Sol-Gel Processing For Inorganic And Organic Composites

Sol-gel processing is reviewed.

Author
H Schmidt
Origin
Institut Fur Neue Materialien Gmbh
Journal Title
Glass Production Technology International 1992 198-201
Sector
Special Glass
Class
S 641

Request article (free for British Glass members)