Sodium Self Diffusion In Glasses And Melts Of The System Na2O-Rb2O-Sio2

Sodium self diffusion was studied from 300 to 1200 degreesC in five glasses and melts of the Na2O-Rb2O-SiO2 system using the radioactive isotope 22Na.