Simas Nmr Investigation Of Atomic Rearrangements During Batch Metling Of Glass

Magic angle spinning nuclear magnetic resonance spectroscopy has been used to investigate atomic rearrangement during the batch melting of a soda-lime-silicate glass.

Author
A R Jones Et Al
Origin
University Of Wales, Uk
Journal Title
Glass Technology 43C 2002 52-55