Silver-Doped 58S Bioactive Glass As An Anti-Leishmania Agent

Bioactive glasses (BG) incorporating antimicrobial agents can be effectively used against microorganisms. In this work, the in-vitro effectiveness of silver-doped 58S BG (BGAg) against Leishmania species was studied.