Servo-Valves Enable Glassmakers To Control Air In The Forming Process

Following the introudction of the third generation of electronic controls for IS lines, Bottero has now gone one step further with the aim of controlling the forming air. In this paper the authors explain what is involved.

Author
N Boglione & C Borsarelli
Origin
Bottero, Italy
Journal Title
Glass 77 5 2000 111-112
Sector
Container glass
Class
C 1544

Request article (free for British Glass members)

Servo-Valves Enable Glassmakers To Control Air In The Forming Process
Glass 77 5 2000 111-112
C 1544