Sensitivity Of Fracture Strength In Porous Glass

This article investigates the effect of porosity and crack size distributions on the fracture behaviour of porous glass through a combined finite element and fracture mechanics method. Simulations showed that the effect of crack size distributions on the change in fracture strength with porosity decreases as the pore size to crack size ratio increases. For a pore size to crack size ratio of

Author
O Keles Et Al
Origin
San Jose State University, California
Journal Title
Int J Appl Glass Science March 2017 116-123
Sector
Special Glass
Class
S 4350