Self-Sustaining Vitrification For Immobilisation Of Radioactive And Toxic Waste

The immobilisation of hazardous (toxic and radioactive) waste using self-sustaining vitrification processes is reviewed.

Author
M I Ojovan & W E Lee
Origin
Sheffield University, Uk
Journal Title
Glass Technology 44 6 2003 218-224
Sector
Special Glass
Class
S 2667