Scientific Research On Speciality Glasses Within The Cnr Project On 'Special Materials For Advanced Technologies' (Italian)

Research activities in progress in five centres within the Italian glass sector of the CNR project are described in detail.

Author
G Scarinci
Origin
University Of Padova, Italy
Journal Title
Riv Staz Sper Vetro 1991 21 5 215 - 220
Sector
Special Glass
Class
S 600