Schott Fires Up 6M Euros Melting Tank

Schott have announced it is ready to start firing up its new melting tank at the Gruneplan (Germany) site, following many months of construction work. The technology group invested around 6M/Euros in the tank, which is equipped with process control technology. It will be used to manufacture premium quality glass products such as Opalika white flashed opal glass, Artista coloured glasses, as well as restoration glass for architectural use.