Ruby Coloured Lead Glasses By Generation Of Silver Nanoparticles

Both yellow and red superficial ruby lead crystal glasses have been obtained by Ag+ ion-exchange. For red ruby colouring lead glass substrates were previously doped with reducing oxides (arsenic, antimony, cerium and tin). The best experimental conditions for silver ion-exchange were determined. The optical absorption behaviour of the samples was studied to point out the influence of the parameters involved in the ion-exchange process. Moreover, other parameters affecting the final colouring of the glasses (kind of dopant, dopant concentration, etc.) were also analysed. The dopant percentage added to the lead crystal glass is the most important factor for developing superficial red ruby colouring. Antimony oxide doped lead glass ion-exchanged with silver showed the most intense red ruby colouring, even for a doping concentration lower than those of arsenic oxide doped samples able to enhance similar colour. Spectral saturation appeared for the highest doping concentration and for the most severe ion-exchange conditions. Chromatic coordinates were calculated from the corresponding transmission visible spectra. The colour purity showed by the samples obtained satisfies the ornamental requirements that motivated this research.

Author
C Gil Et Al
Origin
Fundacion Centro Nacional Del Vidrio, Spain
Journal Title
Materials Chem & Physics 88 1 2004 185-191 Doi: 10.1016/J.Matchemphys.2004.07.006
Sector
Domestic glass
Class
D 1344

Request article (free for British Glass members)

Ruby Coloured Lead Glasses By Generation Of Silver Nanoparticles
Materials Chem & Physics 88 1 2004 185-191 Doi: 10.1016/J.Matchemphys.2004.07.006
D 1344
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.