The Role Of Cr2O3, Lif And Their Mixtures On Crystalline Phase Formation And Microstructure In Ba, Ca, Mg Aluminosilicate Glass

The effect of different additions of the nucleating agents, Cr2O3 and LiF, seperately and as mixtures on the crystallizability, phase assemblages, isomorphism and polymorphism of the crystallizing pyroxenes or celsians, and on the resultant microstructures is investigated.

Author
A A Omar Et Al
Origin
National Research Centre, Cairo, Egypt
Journal Title
Br Ceram Trans J 1991 90 179-183
Sector
Special Glass
Class
S 611