The Relationship Between Regions Of Glass Formation And Pseudoeutectic Regions

A method for calculating pseudoeutectic regions using chemical potentials has been developed. The method can be used not only for calculating the positions of glass formation, but also for comparing glass forming abilities among systems with similar viscous characters.