Refractory Solutions For Extra White Glasses

Extra clear glasses are widely used for solar applications. The extra clear glass properties and especially the higher transmission coefficient induce an evolution of glass furnace running conditions. After discussing the consequences on refractories in terms of corrosion, a new bottom paving solution is proposed. This solution consists of optimally machined fused cast AZS tiles and a new formulation of AZS mortar layer.