Refractories For Glassfibre Melting Furnaces

Refractories specifically designed for glass-contact applications in glass fibre furnaces are discussed with special reference to chromic oxide-containing and zircon-based materials.

Author
C N Mcgarry, T M Wehrenberg
Origin
Corhart Refractories Corp
Journal Title
Glass November 1989 459-461
Sector
Refractories
Class
R 32

Request article (free for British Glass members)

Refractories For Glassfibre Melting Furnaces
Glass November 1989 459-461
R 32