Vlakglas Recycling Nederland is an initiative originally launched by Dutch sheet glass manufacturers. Today, this non-profit organisation has evolved to coordinate all the activities associated with recycling and collecting waste sheet glass throughout the Netherlands. In this article Glass International spoke to Cor Wittekoek from the company about the initiative and how the company has vastly improved the rate of sheet glass recycling in Holland.