Recycling Acid Profitably

The repeated reuse of valuable materials os a goal worth pursuing for a variety of reasons. A Spanish company has developed a process in cooperation with Schott which meets this objective.

Author
J M Rituerto
Origin
General Quimica Sa, Spain
Journal Title
Schott Information No 83/97 18-19
Sector
Special Glass
Class
S 1375

Request article (free for British Glass members)

Recycling Acid Profitably
Schott Information No 83/97 18-19
S 1375