Reaction Of Zirconium Fluoride Monohydrate And Ammonium Bifluoride: Its Effect On Fluoride Glass Preparation And Quality

Ammonium bifluoride and zirconium fluoride monohydrate were reacted prior to glass batching, producing dry ammonium heptafluorozirconate which was used to prepare a high-quality ZBLAN fluoride glass.

Author
K J Ewing Et Al
Origin
Naval Research Laboratory, Washington
Journal Title
J Am Ceram Soc 1989 72 8 1441-1443
Sector
Special Glass
Class
S 305

Request article (free for British Glass members)

Reaction Of Zirconium Fluoride Monohydrate And Ammonium Bifluoride: Its Effect On Fluoride Glass Preparation And Quality
J Am Ceram Soc 1989 72 8 1441-1443
S 305