Properties Of Sic-Whisker Reinforced Glass-Ceramic Composite For Biomedical Application

A silicon carbide-whisker reinforced glass ceramic in the calcia-phosphate-silica system was fabricated by hot pressing. The addition of the whiskers to the matrix glass ceramic increased bending strength and fracture toughness by factors of 3 and 4 respectively.