Properties Of Multicomponent Glasses - A Fast And Novel Algorith

How does a certain amount of a specific oxide influence the properties of a glass or a glass melt? This seemingly simple question, frequently put in various contexts, is most difficult to answer in a general way. In terms of thermo chemistry, it is the question for the chemical potentials of such oxides in an multi component system.