Progress In Nd3+, Er3+, And Yb3+ Doped Laser Glasses At Shanghai Institute Of Optics And Fine Mechanics (Siom)

This paper reviews the progress made on Nd3+, Er3+, and Yb3+ doped laser glasses at SIOM. Key properties of Nd: phosphate and Nd: fluorophosphate (FP) laser glasses are presented and compared with the commercial laser glasses from Hoya and Schott. Also reviewed are properties of four types of Er: phosphate glasses.