Processing Of Insulators With Ion Beams

Potential and current progress in ion beam modification of the surfaces of insulators is discussed.

Author
P D Townsend
Origin
University Of Sussex
Journal Title
Glass Technology 1991 32 1 16-19
Sector
Special Glass
Class
S 480