Preparation Of Yba2Cu3O7-X-Based Superconductors By Means Of Glass-Technological Methods

Samples in the system VBa2Cu3O7-x have been produced by melt processing and subsequent annealing to show the potential use of glass-making procedures for preparing high-temperature superconductors.