Preparation Of Infrared Transmitting Cdf2 Based Mixed Halide Glasses

The influence of substituents on the multiphone absorption edge of cadmium fluoride mixed halide glasses has been studied by using a double beam infrared spectrophotometer and the absorption loss due to multiphonon vibration in the bulk glass determined.

Author
A Jha, J M Parker
Origin
Brunel University, University Of Sheffield
Journal Title
Phys Chem Glasses 1991 32 1 1-12
Sector
Special Glass
Class
S 482