Preparation And Nonlinear Optical Properties Of Quantum-Sized Cucl-Doped Silica Glass By The Sol-Gel Process

The sol-gel process has been applied successfully to the preparation of small-sized copper chloride-doped silica glass with a significant quantum-sized effect.

Author
M Nogami Et Al
Origin
Aichi Institute Of Technology, Nagoya University
Journal Title
J Am Ceram Soc 1991 74 1 238-240
Sector
Special Glass
Class
S 497

Request article (free for British Glass members)

Preparation And Nonlinear Optical Properties Of Quantum-Sized Cucl-Doped Silica Glass By The Sol-Gel Process
J Am Ceram Soc 1991 74 1 238-240
S 497