Preparation And Cu+-Ion-Conducting Properties Of Glasses In The System Cubr-Cu2Moo4-Cu3Po4

Cu+- ion-conducting glasses are prepared in the pseudoternary system CuBr-Cu2MoO4-Cu3PO4, and the ion-conducting properties of the glasses obtained are compared to those of the glasses in the system CuI-Cu2MoO4-Cu3PO4, which contain CuI instead of CuBr.