The Physical Properties Of Na20-Si02 Glasses: Correlations Derived Using A Network Theory Model Developed For Nonlinear Hydrocarbon Polymers

This analogy is tested by applying branching theories to glass systems in an attempt to correlate calculated differences in a hypothetical network structure with corresponding variations in the physical properties of the glass.

Author
J L Plawsky
Origin
Rensselaer Polytechnic, Ny, Usa
Journal Title
Physics & Chem Of Glasses 34 1 1993 1-9
Sector
Special Glass
Class
S 703