Permeability Of Fibre-Containing Refractory Castables

Polypropylene, poly(ethylene terephthalate), cellulose, jute and Nomex fibres were added to high-alumina ultra-low-cement refractory castables, and their green and fired permeabilities were determined.

Author
M D M Innocentini Et Al
Origin
Unknown
Journal Title
Am Ceram Soc Bull 81 7 2002 34-37
Sector
Refractories
Class
R 449