Particle Inhilation And Lead Substitute Toxicity

This article examines particle inhilation - methods of entry, fate of inhaled particles, factors affecting deposition, particle deposition methods, ICRP lung deposition, lung clearance of particles and dissolution. It also looks at alternatives to lead.