Oxy-Fuel Firing: Refractory Challenges And Opportunities

Oxy-fuel firing offers many attractions to the glassmaker, but its use is often difficult to justify financially. Recent developments in high performance crown refractories have the potential to significantly improve the economics and increase the usage of this exciting technology.

Author
G Evans Et Al
Origin
Unknown
Journal Title
Glass 77 5 June 2000 141-142