Nucleation And Crystallization Of A Lithium Aluminosilicate Glass

A ZLAS glass of composition 61Si02.6A1203.10Mg0.6Zn0.12Li20.5Ti02 (mol%) has been prepared by a melting process and investigation as far as cristallization is concerned. Glass-ceramic is easily obtained because glass shows a high tendency to crystallize starting from 700 deg C. The titanates of Mg and Zn develop from the phase-separated glass, soon after Tg, and grow to form nucleation centres for the other crystalline phases. The evolution from phase-separated glass to glass ceramic has been followed by many thermal, diffractometric, spectrosocpic, and microscopic techniques.

Author
L Barbieri Et Al
Origin
Unknown
Journal Title
J Am Ceram Soc 80 12 1997 3077-3078
Sector
Special Glass
Class
S 1594a

Request article (free for British Glass members)

Nucleation And Crystallization Of A Lithium Aluminosilicate Glass
J Am Ceram Soc 80 12 1997 3077-3078
S 1594a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.