Nucleation And Crystallization Of Na2O.2Cao.3Sio2 Glass By Differential Thermal Analysis

The nucleation and crystallisation of a soda-lime-silica glass were studied by DTA, and a curve was obtained by plotting either the reciprocal of the temperature corresponding to the crystallisation peak maximum, or the height of the crystallisation peak, as a function of nucleation temperature.